So I recapped the MLB for the ANS server. There were only 13 SMD caps.. 2 - 10uf 16v, 3 - 100 6v, 8 - 47uf 16v. I've done this on some other 90's machines I have... I am all about preventative maintenance, and I'll just forget and they will dry out or leak at some point. At any rate I replaced them with good quality APX Tantalums. What doesn't make sense is there were other tantalums on the board with the same values... a little larger.. I wonder why Apple used SMD electrolytic?? Is there a reason? Or was it a cost cutting thing?? Any ideas? These are not huge caps so I don't see the issue with using the tantalums.. Most servers use tantalum at least some that I have worked on for reliability I would assume since it is high end. Just wondering about what everyone's feedback on this is....